Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.64 J/cm | 10.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copoly LNP* LUBRICOMP* KL002 is a compound based on Acetal Copolymer resin containing 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 5.64 J/cm | 10.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL002 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 5.64 J/cm | 10.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KL002L Acetal LNP* LUBRICOMP* KL002L is a compound based on Acetal Copolymer resin containing 10% PTFE. Added features of this grade include: Wear Resistant, Low Extractible. |
|||
Izod Impact, Unnotched | 5.65 J/cm | 10.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE... |
|||
Izod Impact, Unnotched | 5.68 J/cm | 10.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP JF008E PES LNP* THERMOCOMP* JF008E is a compound based on Polyethersulfone containing 40% Glass Fiber. Characteristics of this grade are: Easy Molding. |
|||
Izod Impact, Unnotched | 5.66 J/cm | 10.6 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 413 Glass Reinforced, Polycarbonate/Polyester Alloy, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Izod Impact, Unnotched | 5.68 J/cm | 10.6 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D4812 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3230A PP SABIC® PPcompound G3230A is a general purpose, 30% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 109612410 |