Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.67 - 6.41 J/cm | 5.00 - 12.0 ft-lb/in | Average value: 4.30 J/cm Grade Count:11 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |
|||
Izod Impact, Unnotched | 4.54 - 6.41 J/cm | 8.50 - 12.0 ft-lb/in | Average value: 5.52 J/cm Grade Count:10 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Unnotched | 4.81 - 6.41 J/cm | 9.00 - 12.0 ft-lb/in | Average value: 5.94 J/cm Grade Count:4 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Unnotched | 1.01 - 6.41 J/cm | 1.90 - 12.0 ft-lb/in | Average value: 3.16 J/cm Grade Count:40 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Unnotched | 4.27 - 6.41 J/cm | 8.00 - 12.0 ft-lb/in | Average value: 5.29 J/cm Grade Count:10 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Izod Impact, Unnotched | 3.20 - 6.41 J/cm | 6.00 - 12.0 ft-lb/in | Average value: 4.34 J/cm Grade Count:4 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Izod Impact, Unnotched | 1.07 - 6.41 J/cm | 2.00 - 12.0 ft-lb/in | Average value: 3.51 J/cm Grade Count:8 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Izod Impact, Unnotched | 1.72 - 6.41 J/cm | 3.22 - 12.0 ft-lb/in | Average value: 3.71 J/cm Grade Count:20 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |
|||
Izod Impact, Unnotched | 0.907 - 6.41 J/cm | 1.70 - 12.0 ft-lb/in | Average value: 4.10 J/cm Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |