Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.32 J/cm @Thickness 3.18 mm |
8.09 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Izod Impact, Unnotched | 4.32 - 18.7 J/cm | 8.09 - 35.0 ft-lb/in | Average value: 10.6 J/cm Grade Count:15 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Unnotched | 4.32 J/cm | 8.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DE0049P PC (Asia Pacific) LNP* Stat-kon* DE0049P is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. |
|||
Izod Impact, Unnotched | 4.32 J/cm | 8.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP JF006LZZ PES LNP THERMOCOMP* JF006LZZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Extrusion Grade, Low Extractable. |
|||
Izod Impact, Unnotched | 4.32 J/cm @Temperature 23.0 °C |
8.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |
|||
Izod Impact, Unnotched | 4.32 J/cm | 8.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10 LNP* THERMOCOMP* QF004 is a compound based on Nylon 6/10 resin containing 20% Glass Fiber. |
|||
Izod Impact, Unnotched | 4.32 J/cm | 8.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10 (Asia Pacific) LNP* Thermocomp* QF004 is a compound based on Nylon 6/10 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 4.32 J/cm | 8.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DE0049P PC LNP* STAT-KON* DE0049P is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. Electrically Conduct.. |
|||
Izod Impact, Unnotched | 4.32 J/cm @Temperature 23.0 °C |
8.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |
|||
Izod Impact, Unnotched | 4.32 J/cm | 8.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF) LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 4.32 J/cm | 8.09 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 626 Nylon 6/6, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.32 J/cm | 8.09 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Lubrilon® 631 Nylon 6/6, Graphite/Molybdenum Disulfide Filled Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Izod Impact, Unnotched | 4.32 J/cm @Thickness 3.18 mm |
8.09 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® JF-1006 E LE BK8-055 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Features: High Viscosity, Low ExtractablesForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |