Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
North Wood Plastics Polypropylene with 60% Wood Fiber, Molding Grade Data provided by North Wood Plastics, Inc. |
|||
Izod Impact, Unnotched | 0.400 J/cm - NB | 0.749 ft-lb/in - NB | Average value: 8.97 J/cm Grade Count:44 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 240 Rigid PVC, Extrusion Electric channels |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 241 Rigid PVC, Extrusion Various profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 325/2 Rigid PVC, Extrusion Building profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 330 Rigid PVC, Extrusion Various profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 620 Rigid PVC, Extrusion Spiral pipes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RI 54 Rigid PVC, Injection Molding Fittings for building trade - high fluidity |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RI 55 Rigid PVC, Injection Molding Fittings for building trade - high fluidity |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 115 Rigid PVC, Extrusion Lead Free Small tubes for shoes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 316 Rigid PVC, Extrusion Lead Free Indoor profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 325/AM Rigid PVC, Extrusion Lead Free Profiles anti mould |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 330 Rigid PVC, Extrusion Lead Free Profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RL 708 Rigid PVC, Extrusion Corrugated electric pipes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RL 710 Rigid PVC, Extrusion Corrugated electric pipes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RST 171 Rigid PVC, Extrusion Lead Free Various transparent profiles |
|||
Izod Impact, Unnotched | 0.400 J/cm | 0.749 ft-lb/in | ASTM Data |
Styron CALIBRE™ 5051 15 Polycarbonate, 5% Glass Reinforced CALIBRE® 5051 is a 5% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5051 polycarbonate resin exhibits high modulus and excellent dimensional stabili.. |
|||
Izod Impact, Unnotched | 0.400 J/cm | 0.749 ft-lb/in | ASTM Data |
Styron CALIBRE™ 7101 15 Polycarbonate, 10% Glass Reinforced CALIBRE® 7101 is a 10% glass reinforced ignition resistant polycarbonate resin equipped with a mold release package for optimal processing. The CALIBRE 7101 resins exhibit a high modules, excepti.. |
|||
Izod Impact, Unnotched | 0.400 J/cm | 0.749 ft-lb/in | ASTM Data |
Styron CALIBRE™ 7101 8 Polycarbonate, 10% Glass Reinforced CALIBRE® 7101 is a 10% glass reinforced ignition resistant polycarbonate resin equipped with a mold release package for optimal processing. The CALIBRE 7101 resins exhibit a high modules, excepti.. |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds R 316 Rigid PVC, Extrusion Rolling shutters |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds R 316/AS Rigid PVC, Extrusion Antistatic profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 116 Rigid PVC, Extrusion Small tubes for shoes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 121 Rigid PVC, Extrusion Electric pipes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds R 244 Rigid PVC, Extrusion Shutters high modulus low curving |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 224 Rigid PVC, Extrusion Various profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 225/R Rigid PVC, Extrusion Lead Free Rolling shutters |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 235 Rigid PVC, Extrusion Electric channels and profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 236 Rigid PVC, Extrusion Electric channels |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RI 52/C Rigid PVC, Injection Molding Electric fittings |
|||
Izod Impact, Unnotched | 0.400 - 5.34 J/cm | 0.749 - 10.0 ft-lb/in | Average value: 3.00 J/cm Grade Count:18 |
Overview of materials for Polypropylene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app.. |