Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.39 - 6.50 J/cm² @Temperature -40.0 - 30.0 °C |
6.62 - 30.9 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 3.68 J/cm² Grade Count:66 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Charpy Impact Unnotched | 4.50 - 6.50 J/cm² @Temperature -30.0 - -20.0 °C |
21.4 - 30.9 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 5.70 J/cm² Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Charpy Impact Unnotched | 2.00 - 6.50 J/cm² @Temperature -30.0 - -30.0 °C |
9.52 - 30.9 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.16 J/cm² Grade Count:14 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact Unnotched | 2.00 - 6.50 J/cm² | 9.52 - 30.9 ft-lb/in² | Average value: 4.05 J/cm² Grade Count:12 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 2.60 - 6.50 J/cm² | 12.4 - 30.9 ft-lb/in² | Average value: 4.16 J/cm² Grade Count:20 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Charpy Impact Unnotched | 4.00 - 6.50 J/cm² | 19.0 - 30.9 ft-lb/in² | Average value: 5.23 J/cm² Grade Count:10 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 3.00 - 6.50 J/cm² | 14.3 - 30.9 ft-lb/in² | Average value: 5.33 J/cm² Grade Count:3 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 2.10 - 6.50 J/cm² | 9.99 - 30.9 ft-lb/in² | Average value: 4.59 J/cm² Grade Count:15 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Charpy Impact Unnotched | 2.40 - 6.50 J/cm² | 11.4 - 30.9 ft-lb/in² | Average value: 5.20 J/cm² Grade Count:7 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Charpy Impact Unnotched | 2.10 - 6.50 J/cm² @Temperature -30.0 - -30.0 °C |
9.99 - 30.9 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.62 J/cm² Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |