Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Radici Radilon® ARV300 RKC (dry) Nylon 66 Glass-fiber reinforced with heat and hydrolysis resistanceInformation provided by Radici group. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1/XCF/30 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-7830 Polyamide 66, with PTFE, lubricant modified, improved wear resistance, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | |
LATI Latistat 87/28-06 PC Dissipative product based on Polycarbonate (PC). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 V60 Black Z PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR Polyamide reinforced with 60% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Asia Pacific, Europe and No.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific) Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179-1 |
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW200F8 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 45 HWCP 45% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-6H nat PA*-GF60 Product description: Grivory GVL-6H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H na.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-50-4 nat PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GVN-5H black 9915 PA*-GF50 Product description: Grivory GVN-5H is a 50 % glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVN-5H black 9915 PA*-GF50 Product description: Grivory GVN-5H is a 50 % glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Conditioned, 30% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179 |
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Dry) Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |