Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.900 J/cm² - NB | 4.28 ft-lb/in² - NB | Average value: 3.52 J/cm² Grade Count:7 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO Data, Low Temp |
Americas Styrenics Styron® 666D Polystyrene
(discontinued **) STYRON® 666D general purpose polystyrene resin is used in injection molding applications, particularly for medical, pharmaceutical and food uses. It offers excellent clarity, intermediate flow char.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS NOVODUR® KU 2-5300 ABS, Injection Grade
(discontinued **) Injection molding grade, high heat resistance and toughness, low-emission.Applications: Automotive parts, household goods.Information provided by the manufacturer.Novodur is produced by Styrolution .. |
|||
Charpy Impact Unnotched | 0.900 J/cm² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | |
LATI Laticonther 88/10 GR/50 PEEK, 50% Graphite Reinforced High thermal conductivity product based on Polyetheretherketone (PEEK). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PX9406P PPE+HIPS (Asia Pacific) Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 125dc HDT. UL94 V-0 rated. Electrical applications. |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179 |
Styrolution PS 116 N/L GPPS Styrolution PS 116N/L is a general purpose polystyrene grade with excellent flow properties and improved heat resistance.Excellent flow propertiesHigh heat resistanceInformation provided by Styrolut.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179 |
Vyncolit 2940 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. USES: Multi-V pulleys and solenoid covers.Information provided by Vyncolit, a Sumitomo Bak .. |
|||
Charpy Impact Unnotched | 0.900 - 1.10 J/cm² | 4.28 - 5.24 ft-lb/in² | ISO 179 |
Vyncolit G885 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | Notched/Unnotched not specified; ASTM DIN53453 |
Total PPC 4720 WZ Polypropylene, Impact Copolymer ATOFINA 4720 is an impact copolymer. 4720 is characterized by a high fluidity offering a combination of east of processing and good mechanical properties.ApplicationATOFINA 4720 has been formulated.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179 |
Vyncolit G865 Novolac Phenolic Glass fiber filled phenolic molding compound with high mechanical, good thermal and electrical properties. USES: Asbestos-free replacement for die-cast automotive metal parts, e.g. reactors for aut.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9340 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Medical sector: superheated steam sterilization.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9340/5 High-Heat Polycarbonate Transparent and opaque shades possible, easy-to-demold.Applications: Medical sector: superheated steam sterilization.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was s.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9341 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers, indicator and brake light lenses.Information provided by Bayer.As of 1 September 2015, Ba.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9343 High-Heat Polycarbonate, UV-Stabilized Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | |
Covestro Baydur® 40 Polyurethane Rigid integral skin polyurethane foam for lightweight moldings. Sandwich structure gives a high stiffness-to-weight ratio.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience .. |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Starpylen M1000-BK1A987 PP, Carbon Black Starpylen M1000-BK1A987 is a high carbon black load PP resinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179 |
Chi Mei Polyrex® PG-33 Polystyrene Standard grade |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179 |
Chi Mei Polyrex® PG-80N Polystyrene High strength |
|||
Charpy Impact Unnotched | 0.900 J/cm² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |
|||
Charpy Impact Unnotched | 0.900 - 6.40 J/cm² @Temperature -40.0 - -20.0 °C |
4.28 - 30.5 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.77 J/cm² Grade Count:22 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Charpy Impact Unnotched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO Data |
Americas Styrenics Styron® 612 Polystyrene
(discontinued **) STYRON® 612 general purpose polystyrene resin is an easy flow resin with no color additives. When used unmodified for the manufacture of food contact articles STYRON 612 complies with the US Food, .. |
|||
Charpy Impact Unnotched | 0.900 J/cm² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability, good mechanical properties.Application areas: Insulating flanges, sealings, pulleys.Information p.. |