Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4472 PC Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² @Temperature -30.0 °C |
28.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4472 PC Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4472 PC (Asia Pacific) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² @Temperature -30.0 °C |
28.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4472 PC (Asia Pacific) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4472 PC (Europe-Africa-Middle East) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² @Temperature -30.0 °C |
28.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4472 PC (Europe-Africa-Middle East) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² - NB @Temperature -30.0 - 0.000 °C |
28.1 ft-lb/in² - NB @Temperature -22.0 - 32.0 °F |
Average value: 6.45 J/cm² Grade Count:5 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | EN ISO 179/1eU |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² @Temperature -30.0 °C |
28.1 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | |
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Dry) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² @Temperature -30.0 °C |
28.1 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Dry) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |
|||
Charpy Impact Unnotched | 5.91 J/cm² @Temperature -30.0 °C |
28.1 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Dry) Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | ISO 179/1eU |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL BK039 is a 13 % glass reinforced heat stabilized lubricated slightly toughened black polyamide 66 for injection molding. It.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² @Temperature -30.0 °C |
28.1 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL BK039 is a 13 % glass reinforced heat stabilized lubricated slightly toughened black polyamide 66 for injection molding. It.. |
|||
Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Crastin® SK695FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |