Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179 |
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 L-HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 6-8159 Polyamide 12, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | |
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | |
Idemitsu Kosan Xarec® WA 214 SPS, 40% Glass Filled |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | |
Idemitsu Kosan Xarec® WA 214LG SPS, 40% Glass Filled Crystalline Polymer, Glass Filled |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® ST25G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179/1eU |
Lucite International Elvakon® 4474 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15 Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 135 °C, Time 720000 sec |
20.0 ft-lb/in² @Temperature 275 °F, Time 200 hour |
ISO 179/1eU |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 0 Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stabil.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® R AR 218 V30 Nylon 66, 30% glass fiber, DRY Description: TECHNYL® AR 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. It contains recycled materials. This product is available in black .. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | IS0179 |
Zhejiang Juner 201-G0 Flame Resistant Nonreinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | IS0179 |
Zhejiang Juner 201-G20 20% Glass Fibre Reinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | IS0179 |
Zhejiang Juner 301-G25 25% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/30 HWCP 10% Glass Fiber and 30% Glass Sphere Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 CF30 HWCP 30% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 CF40 Polyamide 6 40% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® 101 PBT Resin Unreinforced, good toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179/1eU |
BASF Ultradur S 4090 G4 High Speed Unc. 20% Glass Filled PBT Ultradur S 4090 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled injection molding PBT for industrial parts, rigid tough and dimensional stable applications. |
|||
Charpy Impact Unnotched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179/1eU |
BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Charpy Impact Unnotched | 4.20 - 1000 J/cm² | 20.0 - 4760 ft-lb/in² | Average value: 6.03 J/cm² Grade Count:17 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |