Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.50 - 6.00 J/cm² @Temperature -30.0 - -30.0 °C |
21.4 - 28.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.25 J/cm² Grade Count:2 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 3.00 - 6.00 J/cm² | 14.3 - 28.6 ft-lb/in² | Average value: 4.80 J/cm² Grade Count:5 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Charpy Impact Unnotched | 4.50 - 6.00 J/cm² @Temperature -30.0 - -30.0 °C |
21.4 - 28.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.25 J/cm² Grade Count:4 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Charpy Impact Unnotched | 1.80 - 6.00 J/cm² @Temperature -40.0 - -20.0 °C |
8.57 - 28.6 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.64 J/cm² Grade Count:7 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Charpy Impact Unnotched | 5.00 - 6.00 J/cm² | 23.8 - 28.6 ft-lb/in² | Average value: 5.36 J/cm² Grade Count:5 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Charpy Impact Unnotched | 4.00 - 6.00 J/cm² @Temperature 23.0 °C |
19.0 - 28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/ 1eU |
Raschig Group 3572 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis.. |
|||
Charpy Impact Unnotched | 4.00 - 6.00 J/cm² @Temperature -30.0 - -20.0 °C |
19.0 - 28.6 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.87 J/cm² Grade Count:6 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact Unnotched | 1.00 - 6.00 J/cm² | 4.76 - 28.6 ft-lb/in² | Average value: 3.37 J/cm² Grade Count:31 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact Unnotched | 2.70 - 6.00 J/cm² @Temperature -40.0 - -30.0 °C |
12.8 - 28.6 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.42 J/cm² Grade Count:10 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 6.00 - 6.00 J/cm² @Temperature -30.0 - -30.0 °C |
28.6 - 28.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 6.00 J/cm² Grade Count:1 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 4.00 - 6.00 J/cm² @Temperature -30.0 - 30.0 °C |
19.0 - 28.6 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 5.50 J/cm² Grade Count:7 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 2.70 - 6.00 J/cm² | 12.8 - 28.6 ft-lb/in² | Average value: 3.82 J/cm² Grade Count:12 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Charpy Impact Unnotched | 0.400 - 6.00 J/cm² | 1.90 - 28.6 ft-lb/in² | Average value: 2.56 J/cm² Grade Count:22 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 2.00 - 6.00 J/cm² @Temperature -40.0 - -30.0 °C |
9.52 - 28.6 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.35 J/cm² Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Charpy Impact Unnotched | 1.10 - 6.00 J/cm² | 5.24 - 28.6 ft-lb/in² | Average value: 4.23 J/cm² Grade Count:7 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact Unnotched | 1.10 - 6.00 J/cm² @Temperature -40.0 - -20.0 °C |
5.24 - 28.6 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.55 J/cm² Grade Count:25 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |