Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.00 - 5.00 J/cm²
14.3 - 23.8 ft-lb/in²
Average value: 3.50 J/cm² Grade Count:6
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Charpy Impact Unnotched 1.00 - 5.00 J/cm²
4.76 - 23.8 ft-lb/in²
Average value: 2.69 J/cm² Grade Count:7
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
Charpy Impact Unnotched 2.00 - 5.00 J/cm²
9.52 - 23.8 ft-lb/in²
Average value: 3.67 J/cm² Grade Count:6
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Charpy Impact Unnotched 4.00 - 5.00 J/cm²

@Temperature -30.0 - -30.0 °C
19.0 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.33 J/cm² Grade Count:3
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Charpy Impact Unnotched 5.00 - 5.00 J/cm²

@Temperature -30.0 - -30.0 °C
23.8 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.00 J/cm² Grade Count:4
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Charpy Impact Unnotched 0.400 - 5.00 J/cm²

@Temperature -40.0 - -20.0 °C
1.90 - 23.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 2.36 J/cm² Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Charpy Impact Unnotched 3.00 - 5.00 J/cm²

@Temperature -40.0 - -20.0 °C
14.3 - 23.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.33 J/cm² Grade Count:2
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Charpy Impact Unnotched 5.00 - 5.00 J/cm²

@Temperature -30.0 - -30.0 °C
23.8 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.00 J/cm² Grade Count:1
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Charpy Impact Unnotched 2.00 - 5.00 J/cm²

@Temperature -30.0 - -20.0 °C
9.52 - 23.8 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 4.00 J/cm² Grade Count:11
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Charpy Impact Unnotched 5.00 - 5.00 J/cm²

@Temperature -30.0 - -30.0 °C
23.8 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.00 J/cm² Grade Count:4
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Charpy Impact Unnotched 2.50 - 5.00 J/cm²
11.9 - 23.8 ft-lb/in²
Average value: 3.12 J/cm² Grade Count:5
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Charpy Impact Unnotched 2.80 - 5.00 J/cm²
13.3 - 23.8 ft-lb/in²
Average value: 4.14 J/cm² Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Charpy Impact Unnotched 3.50 - 5.00 J/cm²

@Temperature -40.0 - -30.0 °C
16.7 - 23.8 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 4.05 J/cm² Grade Count:6
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
Charpy Impact Unnotched 2.00 - 5.00 J/cm²
9.52 - 23.8 ft-lb/in²
Average value: 3.80 J/cm² Grade Count:8
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
Charpy Impact Unnotched 2.20 - 5.00 J/cm²
10.5 - 23.8 ft-lb/in²
Average value: 3.55 J/cm² Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Charpy Impact Unnotched 1.90 - 5.00 J/cm²

@Temperature -30.0 - 30.0 °C
9.04 - 23.8 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 3.19 J/cm² Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Charpy Impact Unnotched 2.50 - 5.00 J/cm²
11.9 - 23.8 ft-lb/in²
Average value: 3.50 J/cm² Grade Count:9
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..