Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6 Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² - NB | 28.6 ft-lb/in² - NB | Average value: 9.65 J/cm² Grade Count:4 |
Overview of materials for Nylon 12, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-7847 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Grupo Repol Dinalon® B1S25 G30PV0 30% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 6 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | |
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; .. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler. Colors: GreyAvailable in: Latin AmericaMain Properties: ? Good Mechanical Properties, Good Superficial Aspec.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers KetaSpire® KT-880 GF20 Polyetheretherketone (PEEK), 20% Glass Fiber KetaSpire® KT-880 GF20 is a high flow, 20% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 30.0 °C |
28.6 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® 46HF4130 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GC-4H PA*-CF40 Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-3 X ESD black PA12-GF30 Grilamid LV-3 X ESD black is an antistatic Polyamide 12 for injection molding with 30% glass fiber reinforcement. Main attributes are: antistatic with resistivity < 106 Ohmgood fuel and zinc chlorid.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 30.0 °C |
28.6 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSC-20/4 EC black 9832 PA666-CF20 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 30.0 °C |
28.6 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30/4 PA666-GF30 Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | dry; ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® FRee A3U40G5 25% Glass Filled PA66 FR (Conditioned) Description: Flame retardant without halogens and red phosphorus, 25% glass fiber reinforced injection-molding grade; light colorable; outstanding mechanical and electrical properties.Information pr.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eU |
CENTROPLAST CENTROMID 6.6 CF 20 Polyamide 6.6 carbon fiber This material has very high strength and a high operating temperature. It can be used for precision components, drive parts and housings.Information provided by CENTROPLAST Engineering Plastics GMB.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eU |
CENTROPLAST CENTRODAL TF Polyoxymethylene + PTFE This material is high strength and high heat strength dimensional stability. Applications include racks and annular gears, dimensionally accurate structural components for pumps, and housings and t.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® B 3225 Z 000000 PBT, 20% Glass Fiber
(discontinued **) PBT, 20% glass fibers, injection molding, impact modified |