Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | |
Ineos ABS Lustran® H604 Standard impact strength.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | |
Ineos ABS Lustran® H701 Medium heat resistance, high impact strength. ,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Forsan® 483 Acrylonitrile Butadiene Styrene (ABS) High heat resistant, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Kau.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 50 H2 PA6, DRY Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 BKB086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | |
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | ISO 179 |
BASF Ultraform S 2320 003 UNC Q600 POM Ultraform S2320 003 UNC Q600 is an easy flowing and rapidly freezing injection molding POM grade. Contains a mold release agent. |