Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Europe-Africa-Middle East) Improved flow PC with excellent processability and mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD124R PC (Europe-Africa-Middle East) LEXAN FXD124R is a transparent/translucent low viscosity grade for light diffusion special effects. FDA compliant. Color package may affect performance.This data was supplied by SABIC-IP for the Eu.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD911A PC (Europe-Africa-Middle East) Lexan FXD911A is a flame retardant, medium viscosity grade with release for the special effect appearance Diffusion in various colors. Color package may affect performance.This data was supplied by .. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1162T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE123R PC (Europe-Africa-Middle East) LEXAN FXE123R is a transparent/translucent, UV stabilised low viscosity grade for special effects colors with a fluorescent appearance. Color package may affect performance.This data was supplied by.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1944 PC Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1944 PC (Europe-Africa-Middle East) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LR180R PC (Europe-Africa-Middle East) LR180R is a medium viscosity,release containing multipurpose polycarbonate industrial gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle .. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Asia Pacific) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-8000 Polypropylene Block-Copolymer INNOPOL® CS 2-8000 is a polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8000 is highly suitable for pipe manufacturing where the required.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Dry) Description: Terblend® N NM-19 XP is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearanc.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Akulon® Fuel Lock FL-LP PA6 Low fuel permeation PA6 suitable for use in injection molding/welding of small engine fuel tanks, UV stabilized |
|||
Charpy Impact, Notched | 6.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
30.9 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM EcoPaXX® Q-E7300 PA410-I Tube Extrusion |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature -30.0 °C |
30.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eA |
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature -30.0 °C |
30.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eA |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |