Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nyco NYGLOS® 4W STO105 Wollastonite in Polypropylene Data for polypropylene reinforced with 15% Nyco NYGLOS® 4W STO105 Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3).. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
PolyOne OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH GF5020 PD1 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A HSK (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S 32HS (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S 32HS (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPC 200 E20 Polypropylene Copolymer, Elastomer Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66
(Unverified Data**) Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Dry)
(di The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-2120 20% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-2120 is developed for producing.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BD310MO Polypropylene Copolymer BD310MO is a heterophasic copolymer. This grade is characterized by an optimum combination of good impact strength and very high stiffness. This grade is mildly nucleated to maximize the mechanical.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Unipetrol PP MONSTEN® MA 745 Polypropylene Impact Copolymer Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 935 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 950 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EE188AI Polypropylene TPO Compound Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EE189AI Polypropylene TPO Compound Daplen™ EE189AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
DSM Stanyl® TW242FM10 PA46-(GF+MF)50 50% Glass/Mineral Reinforced, Heat Stabilized |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPHC T8020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A HSK (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S 38F (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis MB350WG Polypropylene Compound, Mineral Filled MB350WG is a 30% mineral filled polypropylene compound intended for injection molding. This material has a very high impact strength while maintaining good stiffness and is easy to process. Applic.. |