Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 2.10 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6/66 GF 50 PA6/66, 50% glass fibre
FeaturesPA 6/66 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-g..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East)
CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPC GF7020 PD2 E15 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
Information provided by Polykemi AB
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID 6 HI-M PA6 with improved impact strength
PA 6 with the content of thermoplastic elastomer. Impacted, for moldings with higher toughness even at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets, protecti..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Zytel® E51HSB NC010 is a high molecular weight, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® K224-G8U (Dry) 43% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6  (Unverified Data**)
Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided ..
Charpy Impact, Notched 2.10 J/cm²

@Temperature -20.0 °C
9.99 ft-lb/in²

@Temperature -4.00 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6  (Unverified Data**)
Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h..
Charpy Impact, Notched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
ISO 179-1A
Gromax ATE70-FN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East)
XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi..
Charpy Impact, Notched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Sax Polymers SAXAMID 136Q32 Nylon 6, Injection Molding Grade
SAXAMID 136Q32 is a high impact-modified polyamide 6 injection-molding-grade.Information provided by SAX Polymers
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Sax Polymers SAXLAC 340Q Acrylonitrile Butadiene Styrene
Saxalac 340Q is an siliconized, UV protected, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tes..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® S223-HG7 (Cond.) 35% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® S223-HG7 Nylon 66-35% Glass Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
DSM Stanyl® TE200F8 PA46-GF40
40% Glass Reinforced, Heat Stabilized, for E&E applications
Charpy Impact, Notched 2.10 J/cm²

@Temperature 22.8 °C
10.0 ft-lb/in²

@Temperature 73.0 °F
Partial Break; ISO 179
ExxonMobil Exxtral™ BMV 301 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, designed for automotive interior application in which good surface finish, high s..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 22.8 °C
10.0 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BNU 013 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior ap..
Charpy Impact, Notched 2.10 J/cm²

@Temperature -40.0 °C
9.99 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Eurotec® Tecodur® PB70 GR20 NL IH PBT 20% glass fiber reinforced, impact modified
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, Conditioned
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® K224-HG8 (Dry) 40% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A ESL128 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified
SAXAMID 236Q33 is a impact-modified polyamide 6.6 injection-molding-grade with very good flow properties and outstanding toughness. Even at low temperatures this grade offers super-tough properties...
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
DSM Stanyl® TS200F6 PA46-GF30
30% Glass Reinforced
Charpy Impact, Notched 2.10 J/cm²

@Temperature 20.0 °C
9.99 ft-lb/in²

@Temperature 68.0 °F
ISO 179/1eA
Polyplastic Armlen® PP GF 30-1EX Polypropylene Copolymer, 30% Glass Fiber
Information provided by PolyPlastic Group.
Copyright © lookpolymers.com All Rights Reserved