Polymer Property : Charpy Impact, Notched = 0.600 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 7 T 13 PA6, 7% glass fibre, 13% mineral filling
FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYblend 90VB PC/ABS-Blend, Flame Retardant
Information provided by Polykemi AB
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PPH GF2020 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB SCANMID 6 B12^ NH9L Nylon 6, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® CS 35FL (dry) Nylon 6/66
Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group.
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB SCANMID 6 B12^ Q40 Nylon 6, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo..
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 2-4120 20% Talc-Filled Polypropylene Block-Copolymer
INNOPOL® CS 2-4120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form as well.INNOPOL® CS 2-4120 is developed for p..
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Unipetrol PE HD LITEN® BB 75 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Unipetrol PE HD LITEN® TB 38 HDPE
Made for tape applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s..
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® K224-G4U (Dry) 23% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® K224-LGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® S223-DH Nylon 66 (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Arnitel® EM740 74 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
Edgew 80x10x4 sp=62; ISO 179/1eA
Eurostar Staramide AK8 PA66, 40% Mineral Reinforced, Injection Molding
Staramide AK8 is a 40% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
Eurotec® Tecomid® NB40 NL E PA 6 lubricated, nucleated
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eA
DSM Akulon® K224-G3-FC NA99001 PA6-GF15
15% Glass Reinforced
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
Edgew 80x10x4 sp=62; ISO 179/1eA
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded
BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
Eurotec® Tecodur® PB70 GR10 NL PBT 10% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer  (Unverified Data**)