Total PPR 7238 Polypropylene, Random Copolymer - Blow Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Blow Molding Grade
Manufacturer Total Atofina
Trade Name PPR
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPR 7238 Polypropylene, Random Copolymer - Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Impact Strength. TOTAL Polypropylene 7238 offers excellent impact strength, clarity and gloss.Lubricated 7238 offers superior core rod release for ease in processing.High Purity. 7238 features minimum taste, odor, and optimum thermal stability for superior color and processability.Regulatory. 7238 has passed USP Class VI testing and complies with all applicable FDA and USDA regulations for food contact applications.Recommended Applications. 7238 is recommended for blow molded containers for food, drug, cosmetic and toiletry applications requiring superior impact strength and clarity.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238, L
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.4 MPa
3390 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Tensile Modulus 0.827 GPa
120 ksi
ASTM D638
Flexural Modulus 0.689 GPa
99.9 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 143 °C
289 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648