Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.00 - 1.33 J/cm | 1.87 - 2.50 ft-lb/in | Average value: 1.16 J/cm Grade Count:4 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Izod Impact, Notched | 0.267 - 1.33 J/cm | 0.500 - 2.50 ft-lb/in | Average value: 0.634 J/cm Grade Count:8 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |
|||
Izod Impact, Notched | 0.374 - 1.33 J/cm | 0.700 - 2.50 ft-lb/in | Average value: 0.655 J/cm Grade Count:27 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Notched | 0.270 - 1.33 J/cm | 0.506 - 2.50 ft-lb/in | Average value: 0.776 J/cm Grade Count:80 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched | 0.267 - 1.33 J/cm | 0.500 - 2.50 ft-lb/in | Average value: 0.536 J/cm Grade Count:76 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.801 - 1.33 J/cm | 1.50 - 2.50 ft-lb/in | ASTM D256 |
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Izod Impact, Notched | 0.801 - 1.33 J/cm | 1.50 - 2.50 ft-lb/in | |
Bulk Molding Compounds BMC 501 Mineral Filled, Glass Fiber Reinforced Compound BMC 501 molding compound is a mineral filled glass-fiber-reinforced compound suitable for compression, transfer and stuffer injection molding. It provides the user with good electrical properties An.. |
|||
Izod Impact, Notched | 0.427 - 1.33 J/cm | 0.800 - 2.50 ft-lb/in | Average value: 0.848 J/cm Grade Count:9 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched | 0.200 - 1.33 J/cm | 0.375 - 2.50 ft-lb/in | Average value: 0.377 J/cm Grade Count:106 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Izod Impact, Notched | 0.340 - 1.33 J/cm | 0.637 - 2.50 ft-lb/in | Average value: 0.705 J/cm Grade Count:22 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Izod Impact, Notched | 0.370 - 1.33 J/cm | 0.693 - 2.50 ft-lb/in | Average value: 0.793 J/cm Grade Count:56 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |