Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.160 - 0.907 J/cm | 0.300 - 1.70 ft-lb/in | Average value: 0.527 J/cm Grade Count:4 |
Overview of materials for PVC, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Notched | 0.910 - 0.910 J/cm @Temperature -40.0 - -40.0 °C |
1.70 - 1.70 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.910 J/cm Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Izod Impact, Notched | 0.430 - 0.910 J/cm | 0.806 - 1.70 ft-lb/in | Average value: 0.649 J/cm Grade Count:26 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.590 - 0.907 J/cm @Temperature -40.0 - -40.0 °C |
1.11 - 1.70 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.730 J/cm Grade Count:3 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.910 - 0.910 J/cm @Temperature -40.0 - -40.0 °C |
1.70 - 1.70 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.910 J/cm Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Notched | 0.374 - 0.908 J/cm | 0.700 - 1.70 ft-lb/in | Average value: 0.662 J/cm Grade Count:25 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |