Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.87 J/cm @Temperature 23.0 °C |
3.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC30P200-01BG 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, General Purpose Black, Blow Molding Grade Applications: Load floorSeat backFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D-256 |
PlastiComp Velocity® LCF40-PA66 High Flow Nylon 66, 40% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LCF30 - PA66 Nylon 66, 30% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 1/8" sample; ASTM D256 |
Albis Plastics PC/PET 748/718 GF 20 HZ 20% Glass Fiber
(discontinued **) Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET)Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical ResistanceApplications: Pump Components, Industrial and.. |
|||
Izod Impact, Notched | 1.87 - 3.20 J/cm | 3.50 - 6.00 ft-lb/in | ASTM D265 |
Alcoa KAMA 3400 Super High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Izod Impact, Notched | 1.87 J/cm @Diameter 3.17 mm |
3.50 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5800 High Impact Polystyrene
(discontinued **) Balance of toughness and rigidity, Good gloss, USP Class VIApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection .. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 73°F; ASTM D256 |
M. Holland Company AB308LG ABS Acrylonitrile Butadiene Styrene High flowGood impact resistanceHigh stiffnessApplications: Household goodsPackagingInformation provided by M. Holland |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF30 IM2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PC/ASA FR1508 UV Availability: North AmericaForms: PelletsAdditive: Flame Retardant and UV StabilizerFeatures: Flame Retardant, Good UV Resistance and Halogen FreeInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Chemlon® 345G Nylon 610, Glass Fiber Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN133GL (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256A |
Dow C702-20 Polypropylene Impact Copolymer Resin OverviewHigh impactComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20 Polypropylene Resin is intended for use in injection molded applications requiring high impact. It is parti.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol BR7039 Nylon 6 Alloy, bondable to TPU Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Engineered Polymer Solutions ABS PCR 400, Recycled General Purpose with 40% Post Consumer ABS. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Aclo Accuguard Polycarbonate POL050G10HIV0L Glass Reinforced High Impact Flame Retardant |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 257 PPO A high flow grade for applications requiring high impact strength, heat resistance and dimensional stability.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 8266 Natural 02 Rigid PVC, Extrusion, Natural 02 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FS-4 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |