Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 5002 CU Natural 50% Filler Content Polypropylene This product is well suited for non-glossy appliance type parts. It replaces ABS at favorable cost performance characteristics and can be made UV stable. This product can be color matched in most c.. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT2600-677UV Thermoplastic Polyolefin, UV Stabilized, 0848 Black Applications: Exterior trimStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4900-745UV Thermoplastic Polyolefin, UV Stabilized, CJM Medium Khaki Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Oxford Polymers Oxnilon 66-15-IMP Impact Modified Nylon 66 for Injection Molding Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 241R PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Internal mold release. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 241S PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Super mold release. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 945AU PC Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8483 PC COPOLYMER (Asia Pacific) Lexan* EXL8483 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 80% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP4REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PC1000 PC (Asia Pacific) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 144R PC (Asia Pacific) LEXAN 144R is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 243R PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL N109-AS Antistatic POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX11355 PC (Asia Pacific) This is a PC based compound with good plating, surface, mechanical performance and flame retardant (Halogen free), a good candidate for Laser Direct Structuring applications. |
|||
Izod Impact, Notched | 8.00 J/cm @Thickness 3.20 mm |
15.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® AL 2647 Polycarbonate, Automotive Lens Injection Grade Easy flowing injection molding grade, UV-stabilized, easy mold release agent.Applications: Automotive lens applications, fulfills U.S. specification SAE J 576C.Information provided by Bayer.As of 1 .. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm |
15.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers PC-1514LUV UV Stabilized Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 8.01 - 9.08 J/cm | 15.0 - 17.0 ft-lb/in | |
Bulk Molding Compounds BMC HT12-1027 Unsaturated Polyester Bulk Molding Compound BMC HT12-1027 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
Nylene® Naxel™ PC41 Polycarbonate Description: Naxel™ PC41 is a 12 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources .. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 243R PC 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |