| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
NYCOA 2366 Plasticized Copolyamide TPE
NYCOA 2366 is an extremely flexible and transparent Nylon copolymer specifically developed for extrusion applications such as high-end fishing line, and flexible tubing. NYCOA 2366 possesses an extr..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS
Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior...
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific)
Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® EXL8134 PC COPOLYMER (Asia Pacific)
Lexan* EXL8134 is a PC/siloxane copolymer resin with high flow, excellent low temperature impact and 30% post consumer recycle content. Limited availability and restricted color only. Higher color v..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® IR2110 PC (Europe-Africa-Middle East)
IR2110 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® PC1000 PC (Asia Pacific)
PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® PC1000R PC (Asia Pacific)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® PC1000R PC (Europe-Africa-Middle East)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® VR2220 PC (Europe-Africa-Middle East)
VR2220 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | Conditioned; ASTM D256 |
|
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**)
Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
|
|||
| Izod Impact, Notched |
8.00
J/cm @Thickness 3.17 mm |
15.0
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Covestro Makrolon® DP1-1243 Polycarbonate, Extrusion
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Izod Impact, Notched |
8.00
J/cm @Thickness 3.17 mm |
15.0
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Kleerdex Kydex® P26 Acrylic/PVC Extrusion Compound
(discontinued **)
High impact profile extrusion compoundApplications: Extruded profiles for recreational equipment, medical equipment, business equipment, profiles for use in the interior of commercial aircraft.Featu..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | Reverse notched; ASTM D256 |
|
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | Reverse notched; ASTM D256 |
|
LG Chemical LUCEL N109-AS Antistatic POM, Unreinforced, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256-03 |
|
Ipiranga Petrochem MB 0310 MDPE
IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | edgewise; ASTM D256 |
|
Haysite 43000 Polyester SMC, 22% Glass Reinforced
The 43000 series sheet molding compound is a general purpose material. Designed for compression molding, this grade exhibits good mechanical properties and resistance to mild corrosive agents.
|
|||
| Izod Impact, Notched |
8.00
J/cm @Thickness 3.20 mm |
15.0
ft-lb/in @Thickness 0.126 in |
ASTM D256 |
|
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, Dry as Molded
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
|
|||
| Izod Impact, Notched |
8.00
J/cm @Temperature 23.0 °C |
15.0
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics PC1000 PC (Europe-Africa-Middle East)
PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics PC1000R PC (Asia Pacific)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched |
8.00
J/cm @Temperature 23.0 °C |
15.0
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East)
PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched |
8.00
J/cm @Temperature 23.0 °C |
15.0
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics PC1003R PC
PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was ..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East)
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP DX11355 PC (Asia Pacific)
This is a PC based compound with good plating, surface, mechanical performance and flame retardant (Halogen free), a good candidate for Laser Direct Structuring applications.
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® V3900WX PBT+PC
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER
PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility
|
|||
| Izod Impact, Notched |
8.00
J/cm @Thickness 3.20 mm |
15.0
ft-lb/in @Thickness 0.126 in |
ASTM D256 |
|
Covestro Makrolon® AL 2647 Polycarbonate, Automotive Lens Injection Grade
Easy flowing injection molding grade, UV-stabilized, easy mold release agent.Applications: Automotive lens applications, fulfills U.S. specification SAE J 576C.Information provided by Bayer.As of 1 ..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
|
|||
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
|
Ashley Polymers Ashlene® P1081 Polycarbonate
A high viscosity resin for blow molding as well as injection molding heavy wall parts requiring maximum impact strength. Also available: P1083, same with UV stabilizer; P1081R, same with release; ..
|
|||