Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Pro® 3012 RC Polypropylene Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Izod Impact, Notched | 0.481 J/cm @Temperature 23.0 °C |
0.900 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Oxford Polymers Oxnilon 66-13GF 13% Glass Fiber Filled Nylon 66 for Injection Molding 13% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 0.481 J/cm @Temperature 22.8 °C |
0.900 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Izod Impact, Notched | 0.481 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.900 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® NJ-000/000 Nylon 12
(discontinued **) Description/Features:General Purpose GradeHeat StabilizedHigh FlowUL 94 HBProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.481 J/cm @Diameter 3.17 mm |
0.900 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos R35C-00 Polypropylene Random Copolymer Grade R35C-00 is a high clarity random copolymer with a high flow rate. This material is designed for high speed injection molding and meets the requirements of the U.S. Food and Drug Administration.. |
|||
Izod Impact, Notched | 0.481 J/cm @Thickness 3.17 mm |
0.900 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 L BK Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackTPCI# 9356102Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.481 J/cm @Thickness 3.17 mm |
0.900 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® POM CO TL10 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.481 J/cm @Thickness 3.17 mm |
0.900 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® TPX-HTN-01033 A 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN213GL (DAM) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.481 J/cm @Temperature 22.8 °C |
0.900 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | molded and tested in accordance with ASTM D 4101; ASTM D256A |
Dow DS6D21 Polypropylene Resin DOW DS6D21 is intended for use in cast film processes. It is particularly suited for applications requiring high clarity.Information provided by DowDow Announced Sale of Global Polypropylene Busine.. |
|||
Izod Impact, Notched | 0.481 J/cm @Temperature 22.8 °C |
0.900 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.481 J/cm @Temperature 22.8 °C |
0.900 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol 6001 HV HSL Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
Ensinger Tecamid® 6/12 Nylon (PA612) Type 6/12 has lower moisture absorption rates than nylon 6/6, hence superior dimensional stability.Information provided by Ensinger, Inc. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy