Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.214 J/cm @Temperature 23.0 °C |
0.401 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers Nemcon™ H ABS DP116P ABS ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM Data |
Americas Styrenics Styron® 613 Polystyrene
(discontinued **) STYRON® 613 high heat, high strength general purpose polystyrene is typically used in applications requiring a clear, tough part such as office products and magnetic media enclosures. It offers goo.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM Data |
Americas Styrenics Styron® 663 Polystyrene
(discontinued **) STYRON® 663 general purpose polystyrene resin is an additive free resin with excellent strength, clarity, and high heat resistance. When used unmodified for the manufacture of food contact articles.. |
|||
Izod Impact, Notched | 0.214 - 1.87 J/cm | 0.401 - 3.50 ft-lb/in | Average value: 0.968 J/cm Grade Count:124 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance .. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Durez® 31906 Phenolic, Injection Grade Durez 31906 Black Phenolic is an asbestos free, medium impact, molding compound. It is designed for applications where additional mechanical strength is required.Information provided by Sumitomo Ba.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Injection Grade Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Compression Grade Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimens.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Injection Grade Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimens.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256A |
Total PPH 3622 Polypropylene, Injection Molding Grade General purpose injection molding and extrusion homopolymerGood Processability -- FINA 3622 is engineered for good processability in thin wall multi- cavity molds.Good Clarity -- FINA 3622 has good .. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256A |
Total PPH 3825WZ Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerNucleation - FINA 3825WZ is engineered with nucleation to provide fast cycle time and improve contact clarity in thin wall multi-cavity molds.Antistat - FINA 3.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256A |
Total PPH 3925WZ Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerNucleation - FINA 3925WZ is nucleated to provide fast cycle time and improve contact clarity.Antistat - FINA 3925WZ contains an antistat that will help protect.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256 |
Plenco 4304 Phenolic, Nodular, Injection Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256A |
Total PPH 3825 Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerEasy Flow - FINA 3825 exhibits exceptionally easy flow characteristics.FDA - FINA 3825 complies with all applicable FDA regulations for food contact applicatio.. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm |
0.401 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPP30-3500F Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.401 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 250 with Lube Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.401 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 260 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.401 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 263 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.401 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 267 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.401 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 268 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.401 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 300 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.401 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 330 BEADS Styrene Acrylonitrile, Transparent Engineering Thermoplastic, High Flow Natural Beads Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.18 mm |
0.401 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Notched | 0.214 - 2.98984 J/cm @Temperature -20.0 - 4.00 °C |
0.401 - 5.60120 ft-lb/in @Temperature -4.00 - 39.2 °F |
Average value: 1.14 J/cm Grade Count:7 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Notched | 0.214 - 0.740 J/cm | 0.401 - 1.39 ft-lb/in | Average value: 0.462 J/cm Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |