Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CA - 42 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CA - 51 HF OG General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 51 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CA - 51 HF OG General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
Plaskolite West Optix® CA-81 General Purpose Acrylic Resin Extrusion Grade Pellets. Highest Molecular weight. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 71 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.160 J/cm @Temperature 22.8 °C |
0.300 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger Sintimid™ V 40% graphite Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Izod Impact, Notched | 0.160 - 0.854 J/cm | 0.300 - 1.60 ft-lb/in | Average value: 0.344 J/cm Grade Count:16 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
M. Holland Company GS230 Polystyrene, General Purpose High heat resistanceGood processabilityHigh strengthApplications: BottlesBusiness equipmentMedical applicationsPackaging |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256-A |
Ineos Styrenics 166H General Purpose Polystyrene (NAFTA) Description: Polystyrene 166H is a high molecular weight general purpose polystyrene with good flow and crystal clarity. Polystyrene 166H offers good processing characteristics while yielding parts .. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
M. Holland Company SA500 Styrene Acrylonitrile High clarityGood processabilityHigh stiffnessApplications: Color concentratesCompounding |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON EX11402 PEI LNP* STAT-KON* EX11402 is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D 638 |
Styrolution PS 1900 GPPS Foam extrusionVery high flowHigh heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 3.17 mm |
0.300 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN®-N 055 SAN resin These are typical values and are not intended for specification purposes. UL approved file No. is E142893. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CA - 75 OG General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
Plaskolite West Optix® CA-61 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Good heat resistance, medium flow. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | 0.5 in.; ASTM D256 |
Resirene Resirene® HF-666 General Purpose Polystyrene Features:High FlowEasy ProcessingHigh ProductivityFDA Rating: 21 CFR 177.1640External Lubrication AvailableApplications:Medium Wall ApplicationsInjectionToysCassette CasesInformation provided by US .. |
|||
Izod Impact, Notched | 0.160 - 0.961 J/cm | 0.300 - 1.80 ft-lb/in | Average value: 0.484 J/cm Grade Count:22 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Izod Impact, Notched | 0.160 - 33.0 J/cm | 0.300 - 61.8 ft-lb/in | Average value: 3.38 J/cm Grade Count:677 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON ME003S PP LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized. |
|||
Izod Impact, Notched | 0.160 - 0.202 J/cm | 0.300 - 0.378 ft-lb/in | Average value: 0.175 J/cm Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |