Mechanical Properties Metric English Comments
Izod Impact, Notched 0.400 - 0.500 J/cm
0.749 - 0.937 ft-lb/in
ASTM D256-06
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Izod Impact, Notched 0.400 - 0.500 J/cm

@Temperature -40.0 - -20.0 °C
0.749 - 0.937 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.168 J/cm Grade Count:1
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.500 - 0.500 J/cm

@Temperature -29.0 - -29.0 °C
0.937 - 0.937 ft-lb/in

@Temperature -20.2 - -20.2 °F
Average value: 0.500 J/cm Grade Count:1
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.300 - 0.500 J/cm

@Temperature -30.0 - 0.000 °C
0.562 - 0.937 ft-lb/in

@Temperature -22.0 - 32.0 °F
Average value: 0.579 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Notched 0.300 - 0.500 J/cm

@Thickness 3.20 - 3.20 mm
0.562 - 0.937 ft-lb/in

@Thickness 0.126 - 0.126 in
Average value: 0.579 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Notched 0.400 - 0.500 J/cm

@Temperature -30.0 - 0.000 °C
0.749 - 0.937 ft-lb/in

@Temperature -22.0 - 32.0 °F
Average value: 0.475 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Notched 0.400 - 0.500 J/cm

@Thickness 3.20 - 3.20 mm
0.749 - 0.937 ft-lb/in

@Thickness 0.126 - 0.126 in
Average value: 0.475 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Notched 0.450 - 0.500 J/cm

@Temperature -30.0 - 0.000 °C
0.843 - 0.937 ft-lb/in

@Temperature -22.0 - 32.0 °F
Average value: 0.475 J/cm Grade Count:1
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Izod Impact, Notched 0.500 - 0.500 J/cm

@Temperature -40.0 - -40.0 °C
0.937 - 0.937 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.500 J/cm Grade Count:1
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
Izod Impact, Notched 0.450 - 0.500 J/cm
0.843 - 0.937 ft-lb/in
ASTM D256
Loxim 330 12V0 Nylon 6
Information provided by Loxim Industries
Izod Impact, Notched 0.400 - 0.500 J/cm
0.749 - 0.937 ft-lb/in
ASTM D256
Loxim 820 12 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 0.400 - 0.500 J/cm
0.749 - 0.937 ft-lb/in
ASTM D256
Loxim 810 01 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 0.400 - 0.500 J/cm
0.749 - 0.937 ft-lb/in
IS 13411-1992
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded
Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit..
Izod Impact, Notched 0.400 - 0.500 J/cm
0.749 - 0.937 ft-lb/in
IS 13411-1992
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color..
Izod Impact, Notched 0.400 - 0.500 J/cm
0.749 - 0.937 ft-lb/in
IS 13411-1992
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded
Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit..
Izod Impact, Notched 0.210 - 0.500 J/cm

@Temperature -40.0 - -40.0 °C
0.393 - 0.937 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.374 J/cm Grade Count:11
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Izod Impact, Notched 0.200 - 0.500 J/cm

@Temperature -18.0 - -18.0 °C
0.375 - 0.937 ft-lb/in

@Temperature -0.400 - -0.400 °F
Average value: 0.325 J/cm Grade Count:4
Overview of materials for Acrylic, Impact Modified Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 0.200 - 0.500 J/cm

@Temperature -18.0 - -18.0 °C
0.375 - 0.937 ft-lb/in

@Temperature -0.400 - -0.400 °F
Average value: 0.275 J/cm Grade Count:4
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..
Copyright © lookpolymers.com All Rights Reserved