Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.350 - 0.450 J/cm | 0.656 - 0.843 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_4310 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Izod Impact, Notched | 0.350 - 0.450 J/cm | 0.656 - 0.843 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_4410 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Izod Impact, Notched | 0.350 - 0.450 J/cm | 0.656 - 0.843 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_4510 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Izod Impact, Notched | 0.350 - 0.450 J/cm | 0.656 - 0.843 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Izod Impact, Notched | 0.300 - 0.450 J/cm @Temperature -40.0 - -20.0 °C |
0.562 - 0.843 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.363 J/cm Grade Count:2 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | 0.163 - 0.450 J/cm | 0.305 - 0.843 ft-lb/in | Average value: 0.363 J/cm Grade Count:12 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.300 - 0.450 J/cm @Temperature -40.0 - -40.0 °C |
0.562 - 0.843 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.375 J/cm Grade Count:1 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Izod Impact, Notched | 0.400 - 0.450 J/cm | 0.749 - 0.843 ft-lb/in | ASTM D256 |
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo.. |
|||
Izod Impact, Notched | 0.400 - 0.450 J/cm | 0.749 - 0.843 ft-lb/in | ASTM D256 |
Loxim 810 02T HB Polypropylene Compound, 10% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.350 - 0.450 J/cm | 0.656 - 0.843 ft-lb/in | ASTM D256 |
Loxim 820 02T V0 Polypropylene Compound, 20% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.350 - 0.450 J/cm @Temperature -40.0 - -40.0 °C |
0.656 - 0.843 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.400 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Izod Impact, Notched | 0.400 - 0.450 J/cm @Temperature -40.0 - -20.0 °C |
0.749 - 0.843 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.425 J/cm Grade Count:1 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |