Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200-30 Polyester SMC Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4181 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EX1632T PC Lexan* EX1632T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and UV stabilizer. It is available .. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8483 PC COPOLYMER (Asia Pacific) Lexan* EXL8483 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 80% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP3AEU PC (Europe-Africa-Middle East) Lexan HP3AEU resin is a medium flow polycarbonate with mold release designed for medical devices and pharmaceutical applications. It is assessed with biocompatible ISO10993 (or USP Class VI) and is.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PC1000 PC (Asia Pacific) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PC1000 PC (Europe-Africa-Middle East) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | Conditioned; ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Asia Pacific) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL N109-HR Heat Resistant POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 8.00 J/cm @Thickness 3.20 mm |
15.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
Izod Impact, Notched | 8.00 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC1000 PC PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
Izod Impact, Notched | 8.00 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC1003R PC (Asia Pacific) PC1003R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched | 8.00 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC1500 PC PC1500 resin is a medium-high flow (MFR = 15 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ISO 180 |
Shanghai Ofluorine 9202F PVDF Powder for cables Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, .. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX11355 PC (Asia Pacific) This is a PC based compound with good plating, surface, mechanical performance and flame retardant (Halogen free), a good candidate for Laser Direct Structuring applications. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC1500 PC (Asia Pacific) PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched | >= 8.00 J/cm | >= 15.0 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 157 Phenolic Molding Long glass fiber Filler, Compression Molded Characteristics:Shock resistant ( High impact strength )Very good mechanical strengthGood dielectric strengthLow water absorptionLow shrinkageColor-pale brown, black, dark brown, green etc.Medium/st.. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ISO 180 |
Shanghai Ofluorine 9201 PVDF Pellets for cables Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, .. |