Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm |
3.71 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trimid® N6-TG30L-BK 30% Glass Fiber, High Impact Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | Approximation; ISO 180/1U |
Albis Plastics Tedur® L V 9400-1 PPS, 15% Carbon Fiber
(discontinued **) High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Clutch Components, BushingsProcessing: Inje.. |
|||
Izod Impact, Notched | 1.98 J/cm @Diameter 3.17 mm |
3.71 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5511 High Impact Polystyrene Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C.. |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm |
3.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF15 IM HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm |
3.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF18 IM 511 18% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 18% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm |
3.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PC TL15 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm |
3.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN®-V 450 ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® N120GL (COND, 50% RH) Nylon 6, 20% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 6510E Injection Molding Polypropylene Impact CopolymerApplications: General purpose injection molding of consumer products, household appliances, lawn and garden items and medical components.Formolene 6510E is a higher impact, medium st.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437C40L Calcium Reinforced |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437M20L Mica Reinforced |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 733LD Nylon 6 A modified injection molding grade nylon for applications requiring flexibility.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 7777 Rigid PVC, Extrusion Georgia Gulf 7777 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SBB 3707 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Medium Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provi.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |