Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.23 J/cm @Temperature 22.8 °C |
2.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-G43 Nylon 66, 43% Glass Reinforced Nylon 66, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Izod Impact, Notched | 1.23 J/cm @Diameter 3.17 mm |
2.30 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5810 High Impact Polystyrene
(discontinued **) Balance of toughness and rigidity, Good gloss, USP Class VIApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection .. |
|||
Izod Impact, Notched | 1.23 J/cm @Temperature -40.0 °C |
2.30 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Butyrate 513E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Global POM-100 High Viscosity Acetal Homopolymer Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Ineos J50-200-178 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the molding of screw caps dedicated to the packaging of carbonated beverages. This material m.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256-A |
Ineos Styrenics Avantra® 2710 High Impact Styrenic Polymer (Global) Description: Avantra® 2710 is a high-impact grade of polystyrene with improved stress crack resistance, developed primarily for extrusion and thermoforming applications, especially for the refrig.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.20 mm |
2.30 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HFH 403 Flame Retarded HIPS Key features: Low flammable V-2 grade. Common Uses: TV and VCR housing.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resis.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 IM 0240 Impact Modified Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Impact ModifierFeatures: High Density and Impact ModifiedProcessing Method: Injection MoldingInform.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 GF30 ML HS 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide LubricantFeatures: Lubricated and Heat StabilizedIn.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Techmer ES Plaslube® J-4/30/TF/13/SI/2 NAT PA6/12 |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PA6 GF20 RM L BK Nylon 6 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Low Moisture Absorption and LubricatedBlackTPCI# 9718102Inf.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 6.35 mm |
2.30 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PlastxWorld CEVIAN® CGF10 10% GF PC/Acrylic Alloy Glass fiber reinforced PC/Acrylic alloy.These are typical values and are not intended for specification purposes. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN133GLUV (DAM) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated, UV Stabilized Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | 0.125 in; ASTM D256 |
Chase Plastics CP Pryme® NN343L (Dry) Nylon 66, 43% Glass Fiber Reinforced, Lubricated, Recycled Content Features: Recycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Washington Penn Medium Impact Copolymer 10% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | |
Zylog Hipolyene® 7635 MI Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.23 J/cm @Temperature -40.0 °C |
2.30 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Butyrate 485A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437G10M20CL Glass/Mineral Reinforced Coupled |
|||
Izod Impact, Notched | 1.23 J/cm @Temperature -40.0 °C |
2.30 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® P270WO PPO An extrusion grade for high temperature applications requiring flame retardancy as well as high mechanical strength and toughness such as electrical housings.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Cheng Yu Plastic A703G25 ABS 25% Glass Fiber Reinforced |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 131 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P6-30FG-0860 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 520-40G Nylon 66, 40% Glass Reinforced A general purpose 40% glass reinforced Nylon 66 resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.18 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® QF-1006 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |