A. Schulman ComAlloy Hiloy® 131 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 131 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 86
86
ASTM D785
Tensile Strength, Ultimate 46.0 MPa
6670 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 164 °C
327 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 225 °C
437 °F
Approximate middle barrel temperature.