Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.17 J/cm @Temperature 23.0 °C |
2.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P261-01 Polypropylene Copolymer, Medium Impact, Black Applications: Radiator grille inlet supportElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | Injection Molding; ASTM D256 |
Network Polymers F7000 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Polymer Resources NY66-IMG13-[color]H Nylon, 13% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature 22.8 °C |
2.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Izod Impact, Notched | 1.17 J/cm @Diameter 3.17 mm |
2.19 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 731G High Impact Polystyrene
(discontinued **) Balance of stiffness and toughness, High impact, USP Class VIApplications: Razor components, Personal care, Consumer goodsIn addition, exposure to gamma radiation in the 2.02-6.06 megarad range ahs .. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1530 compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA 12 (Asia Pacific) LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conductive. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXQ PPA LNP* LUBRICOMP* UFL36SXQ is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15%PTFE. Added features of this material include: Wear Resistant, Heat Stabilized, Bearing Grade. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE GF30 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good UV ResistanceAdditive: UV StabilizerInformation provided by TP Composites.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 NAT001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightUL File Number: E157318Appearance: Black and Natural ColorTPCI# 9475101Information provi.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PBT GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D 638 |
Styrolution PS 5300 HIPS Excellent ESCRFree of zinc additivesMatte, easily decorated finishGood toughnessUL Classification 94 HBInformation provided by Styrolution |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RX10405H PA 66 LNP* Thermocomp* RX10405H is a compound based on Nylon 6/6 containing Carbon Fiber. Characteristics of this grade are: Healthcare. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature 23.0 °C |
2.19 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp ZF-1006 BK8-950 PPE+PS LNP* Thermocomp* ZF-1006 BK8-950 is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature -30.0 °C |
2.19 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 0325 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityTPC# 6066102Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SBF 3779 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 2520A Injection Molding Polypropylene Medium Impact CopolymerApplications: Closures, Housewares, and Small Appliance ApplicationsFormolene 2520A is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Ecomass® 1066ZD96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Technical Polymers |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Aclo Accutech ABS ABS834G10L Glass Reinforced |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 525LD-33G Nylon 66, 33% Glass Reinforced High impact Nylon 66 reinforced with 33% glass fibers, lubricated.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 1420B Polycarbonate, 20% Glass Reinforced A 20% glass reinforced polycarbonate for increased mechanical strength and thermal properties, modified for good impact with increased dimensional stability and overall toughness. 1423B with UV sta.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6 GF25 FR 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Flame RetardantFeatures: Flame Retardant UL File Number: E157318Processing Met.. |