Network Polymers F7000 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Network Polymers F7000 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Ignition RetardantInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Melt Flow 9.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 31.0 MPa
4500 psi
ASTM D790
Flexural Modulus 1.72 GPa
250 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.20 ft-lb/in
Injection Molding; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
ASTM D648
Vicat Softening Point 96.0 °C
205 °F
ASTM D1525
Flammability, UL94 V-0
V-0
0.0625 in
Descriptive Properties Value Comments
Color Stability min 10
Change in E at 300 hours; ASTM D4459