Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. |
|||
Izod Impact, Notched | 1.15 J/cm @Temperature -30.0 °C |
2.15 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
Izod Impact, Notched | 1.15 J/cm @Temperature -30.0 °C |
2.15 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East) XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Izod Impact, Notched | 1.15 J/cm @Temperature -30.0 °C |
2.15 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Izod Impact, Notched | 1.15 - 8.00 J/cm | 2.15 - 15.0 ft-lb/in | Average value: 4.92 J/cm Grade Count:3 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched | 1.15 - 5.97968 J/cm @Temperature -40.0 - 121 °C |
2.15 - 11.2024 ft-lb/in @Temperature -40.0 - 250 °F |
Average value: 2.55 J/cm Grade Count:2 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
Flint Hills P5C4K-089 Random Copolymer Polypropylene Features: Good clarity. Product does not contain animal derived components. Phthalate-freeApplications: Cast FilmInformation provided by Flint Hills Resources. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem MB 0434 LS-L MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem MB 0435 MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
Kuraray Genestarâ„¢ G1302 Nylon, 30% Glass Filled Abrasion Resistance HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It delivers low.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
Kuraray Genestarâ„¢ G1350H Nylon, 35% Glass Filled Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in .. |
|||
Izod Impact, Notched | 1.15 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.15 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA6-RG30 Flame Retardant, 30% Glass Fiber Reinforced PA6 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: Thi.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 9085 PEI Blend High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke and flame evolution. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 9085 PEI Blend (Asia Pacific) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke and flame evolution. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 9085 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 55/55 with low toxicity, smoke and flame evolution. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.15 J/cm @Temperature 23.0 °C |
2.15 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA303G6 Nylon 6.6, Heat Stabilized, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PX01658 PA 6 LNP* Thermocomp* PX01658 is a compound based on Nylon 6 containing Proprietary Fillers. |