Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Oxford Polymers PEI 1000 PEI Product Description: (Unreinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Colors AvailableInformation provided.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced Acrylonitrile Butadiene Styrene, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources ABS-G30 ABS, 30% Glass Reinforced Acrylonitrile Butadiene Styrene, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-M25G15-[color]-H Nylon 66, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 66, 25% Mineral, 15% Glass Reinforced, Lubricated and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.00 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Stat-Tech™ PS-18CF/000 CM Black Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinu Preliminary Data SheetDescription/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
Izod Impact, Notched | 0.534 - 0.747 J/cm | 1.00 - 1.40 ft-lb/in | Average value: 0.614 J/cm Grade Count:4 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® HDPE FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HIPS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 0135 BL069 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF/B40 L 20% Glass Bead/Glass Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by Weight and Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation .. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® TPX-PA6-03034 Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber ReinforcementAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackInformation pro.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PBT GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 MV5 Unreinforced Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256A |
Dow C700-35 Polypropylene Impact Copolymer Resin OverviewHigh stiffnessGood mold fillabilityComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C700-35 Polypropylene Resin is intended for use in injection molding processes where medium .. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA211 Nylon 6, General Purpose Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
LNP ULTEM® SMU5834 Polyetherimide, 20% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |