Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | Injection; ISO 179/ 1eA |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | Injection and Compression; ISO 179/ 1eA |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
Charpy Impact, Notched | 0.150 - 0.300 J/cm² | 0.714 - 1.43 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² @Temperature 23.0 °C |
0.952 - 1.43 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group RALUPOL® 2200 UP Polyester Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets.. |
|||
Charpy Impact, Notched | 0.300 - 0.300 J/cm² @Temperature -20.0 - -20.0 °C |
1.43 - 1.43 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.300 J/cm² Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179/1EA |
Raschig Group 3572 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis.. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | Average value: 0.248 J/cm² Grade Count:4 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² @Temperature -30.0 - -30.0 °C |
0.952 - 1.43 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.250 J/cm² Grade Count:4 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.300 - 0.300 J/cm² @Temperature -40.0 - -40.0 °C |
1.43 - 1.43 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 0.300 J/cm² Grade Count:1 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179 |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179 |
Vyncolit 4221 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179 |
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,.. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179 |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179 |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Charpy Impact, Notched | 0.300 - 0.300 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 1.43 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.300 J/cm² Grade Count:1 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |