Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.70 J/cm² @Temperature 0.000 °C |
8.09 ft-lb/in² @Temperature 32.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific) |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics GELOY HRA170D ASA+PC (Europe-Africa-Middle East) GELOY HRA170D resin is a PC-ASA blend with permanent antistatic behavior. It is typically used in applications that require antidust properties and high impact retention. Geloy HRA170D resin is typi.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANMID 6 B23^ E F30 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas re.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 179/1eA |
SYNTHOS Forsan® 573 L Acrylonitrile Butadiene Styrene (ABS) Increased heat resistant, glossy, UV stabilized.Applications: Electrotechnics, automotiveHousehold appliances, office equipment, car interior parts, profiles, ABS sheets, etc.Synthos was formerly kn.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
Styrolution PS 495F HIPS Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, Conditioned Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Europe-Africa-Middle East) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO Data |
Styron Magnum™ 341 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® TV6 241 T Impact Modified PBT-20% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 HWUVCP Nylon 66, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4108 nat PA612-GF50 Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801AHS BK010 Nylon 66
(Unverified Data**) Super Toughened Heat Stabilized Polyamide 66 Zytel ST801AHS BK010 is a Super Tough high performance black polyamide 66 resin. It offers outstanding molding performance in injection molding applicati.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 30.0 °C |
8.09 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
Dry; ISO 179/Af |
Arkema Group Orgalloy® RS 6600 Polyamide 6.6 Alloy Polyamide Alloy, Rigid grade, Nylon 6.6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | cond.; ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-27 MCS I Polyamide 6 - Impact Modified High impact resistance grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:H.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Conditioned, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO Data |
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8333G HI HS BK-102 is a 33% glass reinforced, impact modified polyamide 6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in c.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G14AHS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS NC010 is a 14% glass fiber reinforced toughened high flow heat stabilized polyamide 66 resin. It offers outstanding perform.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Laser Markable Polyamide 66 Zytel LM70G35HSLX is a 35% glass fiber reinforced heat stabilized lubricated polyamide 66 for injection molding. It is well suited fo.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX2355 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2355 is an unfilled, medium heat, low odour and low emission material with excellent heat aging performance. It has been developed for automotive interior applications, such as instrument pa.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | |
Polimeri Europa SINKRAL C423/M3 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,95-08-16-15 Special low gloss grade for injection moulding. Good impact resistance coupled with good flow permi.. |