Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66 Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergamid™ A70 G25 U-SO TM Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Nilit FRIANYL A63 HH Nylon 6.6 for injection molding Nylon 6.6 for injection molding, heat and hydrolysis stabilizedInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 W-KV20 Nylon 6 for injection molding, 20% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1105-7751 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature -20.0 °C |
3.33 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
IRPC Polimaxx Polene 2300K Polypropylene Block Copolymer CHARACTERISTICS: HIGH IMPACTAPPLICATIONS: INJECTION MOLDING FOR FURNITURE, HOUSEWARES, CLOSURES, CONTAINERS, AUTOPARTS AND ELECTRICAL APPLIANCES |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, DRY Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179-1 |
Unitika M1030DH PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40 Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HTV-3H1 nat PA6T/6I-GF30 Product description: Grivory HTV-3H1 natural is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45 Product description: Grilon TSC-30/4 LF 15 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers and 15% of a combination of PTFE and silicone oil. Grilon .. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 500TE NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500TE NC010 (formerly DE20560) is a medium viscosity toughened acetal homopolymer with very low VOC emissions. Processing.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® GV-2 FWA black 9225 PA*-GF20 Product description: Grivory GV-2 FWA black 9225 is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copoly.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-3 FWA nat PA6T/6I-GF30 Product description: Grivory HT1V-3 FWA natural is a 30 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® MB 3501 Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11-HI,MHL,22-004Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wi.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | |
BASF Novolen® 2340 P Polypropylene Grade with nucleating agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179 |
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30 Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY bl.. |