Designation ISO 1874-PA11-HI,MHL,22-004Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wide range of temperature. Good chemical resistance.Example applications: Tubes for air brake system. approved by ISO 7628, DIN 73378 (PA11-PHLY), NFR 12632, SAEJ 844.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.0 MPa
4790 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 32 %
32 %
50 mm/min
Tensile Modulus 0.610 GPa
88.5 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 5.50 J/cm²
26.2 ft-lb/in²
0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 138 µm/m-°C

@Temperature 20.0 °C
76.7 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F