Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS (Asia Pacific) High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS (Asia Pacific) PC/ABS with high stiffness and impact performance |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS PC+ ABS General Purpose Non-FR |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East) PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging. |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANLON A 5005B UV PA/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Asia Pacific) CY5100 is a Flame retardant PC blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179-1/1eA |
Styron INSPIREâ„¢ TF0808S(U) Polypropylene TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins. INSPIRE TF0808S for painted parts INSPIRE .. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® XD1575S PBT+PC (Europe-Africa-Middle East) XENOY XD1575S is a high flow PC+PBT blend with good impact properties and good resistance to occasional solvent and gasoline contact. XENOY XD1575S has been specially developed for coated exterior b.. |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Covestro Makroblend® KU 2-7912 MBS151 Polycarbonate + PBT, Impact Grade (PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedAs of 1 September 2015, Bayer MaterialScience was separated.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW341 (COND) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW441 (COND) Nylon 46 High Viscosity, Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature 30.0 °C |
21.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature 30.0 °C |
21.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60 Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TSZ 1 PA666 Product description: Grilon TSZ 1 is a heat stabilized, normal viscosity, impact modified PA66 + PA6 injection molding grade. Grilon TSZ 1 has the following important properties: Excellent flow beha.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 178 |
Ensinger Tecapeek® ID Metal Detectable Polyetheretherketone Tecapeek™ ID metal detectable polyetheretherketone, made from Victrex® PEEK 450G polymer, is formulated to reduce the risk of product contamination and allow for easy detection of fragments in the.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60 Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory.. |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature 30.0 °C |
21.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60 Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PC/ABSz-4 Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |