Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.50 - 4.00 J/cm²

@Temperature 23.0 °C
11.9 - 19.0 ft-lb/in²

@Temperature 73.4 °F
depending on color; ISO 179/1eA
PolyOne Bergamid™ A70 GK30 H Polyamide 66 (Nylon 66)
Information provided by PolyOne
Charpy Impact, Notched 0.360 - 4.00 J/cm²
1.71 - 19.0 ft-lb/in²
Average value: 1.37 J/cm² Grade Count:17
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Charpy Impact, Notched 0.600 - 4.00 J/cm²
2.86 - 19.0 ft-lb/in²
Average value: 2.02 J/cm² Grade Count:113
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Charpy Impact, Notched 0.550 - 4.00 J/cm²
2.62 - 19.0 ft-lb/in²
Average value: 1.64 J/cm² Grade Count:8
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Charpy Impact, Notched 0.600 - 4.00 J/cm²
2.86 - 19.0 ft-lb/in²
Average value: 2.15 J/cm² Grade Count:21
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Charpy Impact, Notched 3.00 - 4.00 J/cm²
14.3 - 19.0 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR N 4303 Bulk Molding Compound
Mechanical high grade standard product.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion p..
Charpy Impact, Notched 0.300 - 4.00 J/cm²

@Temperature -30.0 - -20.0 °C
1.43 - 19.0 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 1.34 J/cm² Grade Count:7
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Charpy Impact, Notched 0.400 - 4.00 J/cm²

@Temperature -30.0 - -20.0 °C
1.90 - 19.0 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 2.71 J/cm² Grade Count:14