Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.20 J/cm² @Temperature 23.0 °C |
15.2 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S ERV3808K (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | |
Ineos ABS NOVODUR® KU 2-5300 ABS, Injection Grade
(discontinued **) Injection molding grade, high heat resistance and toughness, low-emission.Applications: Automotive parts, household goods.Information provided by the manufacturer.Novodur is produced by Styrolution .. |
|||
Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | |
Ineos ABS Lustran® 488 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 3.20 J/cm² @Temperature 0.000 °C |
15.2 ft-lb/in² @Temperature 32.0 °F |
80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig.. |
|||
Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | ISO Data |
Styron Magnum™ 2630 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | Conditioned; ISO 179/1eA |
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6 Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | Bayer Test |
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 55 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Charpy Impact, Notched | 3.20 J/cm² @Temperature 23.0 °C |
15.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVZ 30 HWCP 30% Glass Fiber Z-Qualities Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 3.20 J/cm² @Temperature 23.0 °C |
15.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000/42 CP Nylon 6, Polymer Modified, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 3.20 J/cm² @Temperature 23.0 °C |
15.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000/51 GV 30 HWCP 30% Glass Fiber Nylon 6, Low Temperature Impact Modified, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 3.20 J/cm² @Temperature 23.0 °C |
15.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600/50 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-709 ABS Super impact |
|||
Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-747R ABS - Extrusion Attach case and refrigerator |
|||
Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | |
BASF Luranyl® KR 2420 Polyphenylene Ether + Styrene-Butadiene Blend Grade with high resistance to heat deformation and outstanding impact strength. For auto parts such as air vents or the instrument panel; also used for door-mirror housings.Data was collected by IS.. |
|||
Charpy Impact, Notched | 3.20 J/cm² @Temperature -30.0 °C |
15.2 ft-lb/in² @Temperature -22.0 °F |
|
BASF Luranyl® KR 2420 Polyphenylene Ether + Styrene-Butadiene Blend Grade with high resistance to heat deformation and outstanding impact strength. For auto parts such as air vents or the instrument panel; also used for door-mirror housings.Data was collected by IS.. |
|||
Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | |
Ineos ABS Lustran® QE 1122, Injection Grade
(discontinued **) Injection molding grade, very high impact combined with high modulus, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEO.. |
|||
Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | ISO 179/1eA |
CENTROPLAST CENTROLEN PP LF Polypropylene conductive This material is a low density, easily machined plastic that can be welded and has good surface conductivity. Applications include filter heads and housings, conveyor equipment for flammable liquid.. |