Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 923 PC (Europe-Africa-Middle East) LEXAN 923 is a low viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 50/TF/15/GY04 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179 |
Iran Petrochemical (PCC) BL5 HM 7746 High Density Polyethylene BL5 (HM 7746) is a high density polyethylene with Butene-1 as comonomer. It is a high molar mass, very good impact strength and optimum stress cracking resistance.Applications: large containers abov.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX6120 PPE+PS Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styron CALIBREâ„¢ 2061-15 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-15 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-15 provides excellent heat resistance, impact strength.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® XD1588 PBT+PC (Europe-Africa-Middle East) PBT+PC blend for painted automotive exterior applications, having good flow. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | |
Sibur Discar-L PC/ABS Compositional Polymer Composition material PC/ABS with high shock resistance, thermal, light, and atmospheric resistance for structural parts of technical purpose and parts for internal finishing of automobiles. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179 |
Polyram Polytron P50N07 Polypropylene, 50% Long Glass Fiber, UV Stabilized A chemically coupled 50% long glass fiber reinforced natural polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact, Notched | 2.50 - 3.00 J/cm² | 11.9 - 14.3 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1100 Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179 |
Total PPC 4640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4640 is a nucleated copolymer. PPC 4640 is characterized by good stiffness and impact resistance coupled with high creep resistance. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 30.0 °C |
11.9 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® ELX 40 HNZ TPA Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 30.0 °C |
11.9 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-40/4 FA black 9840 PA666-GF40 Product description: Grilon TSGL-40/4 FA black 9840 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 FA black 9840 is characterized by th.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 5052 (BGZ-15 FC) PA6-GF15 Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilit.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40 Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 30.0 °C |
11.9 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40 Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® RS LC1201 BK040A Nylon 1010
(Unverified Data**) Toughened Renewably Sourced Medium Viscosity Polyamide 1010 Developed for Extrusion Zytel RS LC1201 BK040A is a renewably sourced polyamide 1010 resin containing a minimum of 85% renewably sourced i.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179 |
Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer Injection Molding, High rigidity |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | |
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | |
BASF Luranyl® KR 2402 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade Base grade with a balanced combination of impact strength and stiffness for parts calling for good heat deformation resistance (e.g. warm-air vents, coil formers, sheet and wheel covers).Data was co.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |