Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 51 N PP, basic type FeaturesModified homopolymer PP for injection moulding. General use in all industry branches - packing material, garden flowerpots, toys, furniture industry, hinges, fasteners, clamps, office chairs.. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPC T25020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 H-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | >= 0.500 J/cm² @Temperature 23.0 °C |
>= 2.38 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
Qualchem Danamid FES Polyamide 6 Impact resistant, dryInformation provided by Qualchem Zrt. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/1eA |
Radici Radilon® CAHS (dry) Copolyamide 66/6 General purposeInformation provided by Radici group. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 K Nylon 6.6 for injection molding Nylon 6.6 for injection molding, formulated for the coloration of button baths.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 V0 G5 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 FK 1020 Nylon 6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Charpy Impact, Notched | 0.500 - 4.30 J/cm² | 2.38 - 20.5 ft-lb/in² | Average value: 1.99 J/cm² Grade Count:34 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1850/TF/30 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 179 eA |
Lehmann & Voss LUVOCOM® AC-80/TF/22/BK Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific) NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Terluran® HH-112 ABS Terluran HH-112 is an injection molding grade of ABS with very high heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ EE015U TPO Compound Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Sorona® 3301V BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301V BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight .. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAFORM C 3090(K) POM Copolymer, 27% glass fiber reinforced POM-GF27Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | |
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179 |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
Charpy Impact, Notched | 0.500 - 1.50 J/cm² | 2.38 - 7.14 ft-lb/in² | Average value: 0.867 J/cm² Grade Count:6 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Later 4-V0 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L.. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® T06 204 SN PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |