Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 |
Polycasa AKRYLON XT PMMA AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT .. |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 |
Nilit FRIANYL A63 HH-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 |
Nilit FRIANYL A63 H-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 |
Nilit FRIANYL A63 W-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 |
Nilit FRIANYL B63 KV40 Nylon 6 for injection molding, 40% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 |
Nilit FRIANYL B63 H-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 |
Nilit FRIANYL B63 H-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 |
Nilit FRIANYL B63 HH-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 175 - 239 MPa | 25400 - 34700 psi | Average value: 204 MPa Grade Count:7 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 (H 961-30) |
Lucite International Diakon® CLG356 Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 175 MPa @Load 36.5 kg, Time 30.0 sec |
25400 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® 388 S SAN Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 |
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he.. |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | DIN 2039 |
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | DIN 2039 |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | H 358/30; ISO 2039; DIN 53456 |
Zell-Metall Engineering Plastics Zellamid 250 GF 30 (PA6.6 + 30% glass fiber) Zellamid® 250 GF 30 (PA 6.6 + 30% Glassfibre, black) is the registered trademark for Zell-Metalls 30% glass fiber reinforced nylon grade 6.6. It offers increased strength, stiffness, creep res.. |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSK-30/4 PA666-GB30 Product description: Grilon TSK-30/4 is a heat stabilized, normal viscosity PA66 +PA6 injection molding grade with 30% glass beads. Grilon TSK-30/4 has the following important properties: Good surfa.. |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4105 black 9992 PA610-GF50 Product description: Grilamid XE 4105 black 9992 is a 50% glass fiber reinforced, heat stabilized and UV resistant polyamide 610 (PA610) injection molding grade. This product is to a large extent ba.. |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4108 black 9992 PA612-GF50 Product description: Grilamid XE 4108 black 9992 is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorpti.. |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | Average value: 175 MPa Grade Count:3 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Ball Indentation Hardness | 175 MPa | 25400 psi | ISO 2039-1 |
Lucite International Diakon® CLG357 Acrylic Polymer Information provided by Lucite International |