Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO2039.1 DIN.53456 |
Omnia Plastica Akulon® PA 66.6 Akulon GX - Dry Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tool.. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Nilit FRIANYL A63 FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Nilit FRIANYL A63 GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Nilit FRIANYL A63 GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Nilit FRIANYL A63 H-SG50 Nylon 6.6 for injection molding, 50% mineral filled Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Nilit FRIANYL A63 W-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Nilit FRIANYL B63 SG-GV 2515 Nylon 6 for injection molding, 25% mineral filled and 15% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Nilit FRIANYL C73 H-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Nilit FRIANYL A63 H-GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Nilit FRIANYL A63 KV25 Nylon 6.6 for injection molding, 25% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Quadrant EPP Nylatron® MD PA 6 + metal detectable additive, extruded (ISO Data) Metal detectable 6SA grade High wear and fatigue resistance Lower moisture absorption than standard PA6 Metal and visual detection by blue colour Detection by x-ray also possible Continuous use temp.. |
|||
Ball Indentation Hardness | 170 - 190 MPa | 24700 - 27600 psi | Average value: 179 MPa Grade Count:21 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039 |
GEHR Plastics PET Polyethylene Terephthalate Polyethylene terephthalate shows high tensile and mechanical strength, hardness and toughness, low friction and a high dimensional stability. PET may be used at temperatures ranging from -20°C to.. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
Lucite International Diakon® CLG340 Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Dry Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMINEX® 2000 Cotton Fabric, Phenolic Resin Impregnated, Coarse Application: rollneck-bearings, coverts for friction rollsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30 Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p.. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-15 PA6-GF15 Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b.. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-30 EC PA6-GF30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BGZ-30/2 PA6-GF30 Product description: Grilon BGZ-30/2 is a heat stabilized and impact modified PA6 injection molding grade with 30% glass fibers. Grilon BGZ-30/2 has the following important properties: Good impact s.. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BM-30 PA6-MD30 Product description: Grilon BM-30 is a 30% mineral reinforced PA6 injection moulding grade. Grilon BM-30 has the following important properties: heat stabilizedimpact resistantisotropic shrinkagelig.. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSM-30 PA666-MD30 Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface.. |
|||
Ball Indentation Hardness | 170 - 200 MPa @Time 30.0 sec |
24700 - 29000 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PA 46 Nylon 46 PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality app.. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic .. |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROLYTE FG Polyethylene terephthalate, Food Grade This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance.Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Ball Indentation Hardness | 170 MPa | 24700 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTRO HPM Polyetherimide This material has high strength and rigidity at high temperatures, with good electrical properties. Applications include electrical insulators, and load-bearing components.Information provided by C.. |