Mechanical Properties Metric English Comments
Ball Indentation Hardness 82.0 MPa
11900 psi
DIN 53456
Global PP-2340-TC Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-electrical appliances, bases, panels, auto parts, cupsInformation provided by Global Polymers Corp..
Ball Indentation Hardness 82.0 MPa
11900 psi
H385/30; ISO 2039
Borealis Daplen™ FS65T20 Polypropylene Compound 20% Mineral Filled, Detergent Resistant
Daplen FS65T20 is a 20% mineral filled polypropylene compound intended for injection molding. FS65T20 has been developed especially for applications requiring high detergent resistance and heat sta..
Ball Indentation Hardness 82.0 MPa
11900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® 2S 20 nat PA610
Product Description: Grilamid 2S 20 natural is an unmodified medium viscosity polyamide 610 (PA610), designed for injection molding as well as extrusion. It is characterized by the following product..
Ball Indentation Hardness 82.0 MPa
11900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® XE 4073 nat PA610
Product description: Grilamid XE 4073 natural is a unreinforced, heat and UV stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw materi..
Ball Indentation Hardness 82.0 MPa
11900 psi
H358/30; ISO 2039-1
Chi Mei Polylac® PA-765B ABS - Flame Retardant
F.R. Medium Impact
Ball Indentation Hardness 82.0 MPa
11900 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 200 HI4 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 82.0 MPa
11900 psi
DIN 53456
Ineos Nova S-3207 Medium Impact Compact Polystyrene  (discontinued **)
High flow medium impact polystyrene, designed of injection molding of low friction household goods, packaging and toys. It combines low friction properties with excellent (ultrasonic) weldability.A..