Ball Indentation Hardness 154 MPa

@Load 36.5 kg,
Time 30.0 sec
22300 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultrason® E 2010 MR SW 10111 PESU
Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF
Ball Indentation Hardness 154 MPa

@Load 36.5 kg,
Time 30.0 sec
22300 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultrason® E 3010 MR UN PESU
Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat..
Ball Indentation Hardness 154 MPa
22300 psi
ISO 2039-1
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
Ball Indentation Hardness 154 MPa
22300 psi
ISO 2039-1
BASF Ultrason E 2010 PES
Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Ball Indentation Hardness 154 MPa
22300 psi
ISO 2039-1
BASF Ultrason E 3010 PES
Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance.
Ball Indentation Hardness 154 MPa

@Load 36.5 kg,
Time 30.0 sec
22300 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultrason® E 2010 HC PESU
Information provided by BASF
Ball Indentation Hardness 154 MPa

@Load 36.5 kg,
Time 30.0 sec
22300 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultrason® E 2010 SW Q31 10088 PESU
Information provided by BASF
Ball Indentation Hardness 154 - 224 MPa
22300 - 32500 psi
Average value: 174 MPa Grade Count:12