Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D5420 |
RheTech Products F43-01B 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Drip trayFunctional supportsA/C housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D5420 |
RheTech Products F49-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Fan shroudsSupport ductsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D5420 |
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D5420 |
RheTech Products M25UVP250-01 25% Mica Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsCowl screensRigid exterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D5420 |
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D5420 |
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D5420 |
RheTech Products F35-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Interior trimUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D5420 |
RheTech Products G30P100-00 30% Glass Fiber Reinforced Polypropylene, Natural Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.565 - 21.7 J | 0.417 - 16.0 ft-lb | Average value: 4.47 J Grade Count:22 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D3029 |
Plastics Group Polifil® T-40 40% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D3029 |
Plastics Group Polifil® T-10 10% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D3029 |
Plastics Group Polifil® T-20 20% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Gardner Impact | 0.565 J | 0.417 ft-lb | ASTM D3029 |
Plastics Group Polifil® T-30 30% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Gardner Impact | 0.565 - 33.9 J | 0.417 - 25.0 ft-lb | Average value: 5.46 J Grade Count:32 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Gardner Impact | 0.565 - 13.6 J | 0.417 - 10.0 ft-lb | Average value: 2.05 J Grade Count:32 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |